Steel Grade | C | Si | Mn | Cr | Mo | V | P | S |
H10/SKD7/1.2365/4Cr5Mo2V | 0.35-0.45 | 0.8-1.25 | 0.2-0.7 | 3-3.75 | 2-3 | 0.25-0.75 | ≤0.03 | ≤0.03 |
1.2367/4Cr5Mo3V | 0.35-0.4 | 0.3-0.5 | 0.3-0.5 | 4.8-5.2 | 2.7-3.2 | 0.4-0.6 | ≤0.03 | ≤0.02 |
H11/SKD6/1.2343/4Cr5MoSiV | 0.33-0.43 | 0.80-125 | 0.20-0.60 | 4.75-5.50 | 1.10-1.60 | 0.30-0.60 | ≤0.03 | ≤0.03 |
H12/SKD62/X35CrWMoV5/1.2605/4Cr5MoWVSi | ||||||||
H13/SKD61/1.2344/4Cr5MoSiV1 | 0.32-0.45 | 0.08-1.20 | 0.20-0.50 | 4.75-5.50 | 1.10-1.75 | 0.80-1.20 | ≤0.03 | ≤0.03 |
H21/SKD6/1.2531/SKD5/3Cr2Mo8V | 0.32-0.42 |
0
.8-1.2 |
≤0.5 | ≤0.03 | ≤0.02 | 0.3-0.5 | ≤0.03 | ≤0.02 |
4CrNi4Mo/T23504/SKT6/45NiCrMo16/1.2767 | 0.4-0.5 | 0.1-0.4 | 0.2-0.5 | 1.2-1.5 | 0.15-0.35 | - | ≤0.03 | ≤0.03 |
3Cr2W8V | 0.26-0.36 | 0.15-0.50 | 0.15-0.40 | 3.00-3.75 | - | 0.30-0.60 | ≤0.030 | ≤0.030 |
P20+Ni/SKD6/1.2738/3Cr2NiMo | 0.32-0.40 | 0.20-0.40 | 1.10-1.50 | 1.70-2.00 | 0.25-0.40 | - | ≤0.030 | ≤0.030 |
3Cr2Mo | 0.28-0.40 | 0.28-0.80 | 0.610-1.00 | 1.40-2.00 | 0.30-0.55 | - | ≤0.030 | ≤0.030 |
SKD11/Cr12Mo1V/D12/D11 | 1.4-1.6 | ≤0.40 | ≤0.60 | 11.0-13.0 | 0.80-1.20 |
0.20-0
.50 |
≤0.030 | ≤0.030 |
Cr12Mo1V1/D2/1.2379/ Cr12Mo1V1 | 1.40-1.60 | ≤0.60 | ≤0.60 | 11.00-13.00 | 0.70-1.20 | 0.5-1.10 | ≤0.030 | ≤0.030 |
Cr12/D3/SKD1/1.2080 | 1.9-2.2 | 0.1-0.6 | 0.2-0.6 | 11.00-13.00 | - | -- | ≤0.030 | ≤0.030 |
1.2363/A2/SKD12/Cr5Mo1V | 0.95-1.05 | 0.10-0.40 | 0.40-0.80 | 4.80-5.50 | 0.90-1.20 | 0.15-0.35 | ≤0.003 | ≤0.003 |
5Cr4Mo3SiMnVA1/T23364 | 0.35-0.45 | 0.8-1.1 | 0.8-1.1 | 1.3-1.5 | 0.4-0.6 | 0.2-0.4 | ≤0.030 | ≤0.030 |
4CrMnSiMoV/T23364 | 0.35-0.45 | 0.8-1.1 | 0.8-1.1 | 1.3-1.5 | 0.4-0.6 | 0.2-0.4 | ≤0.030 | ≤0.030 |
Tempering | tool steels are tempered at 482-593°C (900 to 1100°F) for a Rockwell C hardness of 28 to 34. |
Annealing |
Annealing takes place at 760-788°C (1400 to 1450°F) and then the steels are cooled slowly in the furnace at a temperature less
than 4°C (40°F) per hour. |
Cold Working |
tool steels are capable of being readily cold worked by using conventional tooling methods with the alloy in the annealed
condition. |
Welding | Conventional methods are used for welding of P20 tool steels. |
Forging |
tool steels are forged at 1093°C (2000°F) down to 899°C (1650°F). Forging below 871°C (1600°F) is not recommended for these
steels. |
Forming | tool steels can be readily formed by conventional methods in the annealed condition. |
Machinability | tool steels have excellent machinability at about 80% that of water hardening steels. |
Heat Treatment |
tool steels are heated to 871-899°C (1600-1650°F) in the carburizing medium during the carburizing process. After being
carburized, these steels are heated to 816-871°C (1500-1600°F) in order to be hardened and then held for 15 minutes and finally oil quenched. |
Applications | tool steels are used for low-temperature applications that include injection molds and die casting dies. |
1. Who are we?
Our headquarter is located in Shandong, China. Since 2023, we have sold to North America (60.00%), Western Europe (14.00%) and South America (6.00%). There are about 11-50 people in our office.
2. How do we guarantee quality?
Always provide pre-production samples before mass production;
Always carry out final inspection before shipment;
3. What can you buy from us?
Copper, aluminum, die steel, titanium, customized machine parts
4. Why should you buy from us instead of other suppliers?
The company has 25 years of production experience. It has advanced precision production equipment, modern large warehouse, 200000 tons of inventory goods and a number of long-term stable cooperative customers.
5. What services can we provide?
Accepted delivery conditions: FOB, CFR, CIF, EXW
Accepted payment currency: US dollar, Euro, Japanese yen, Canadian dollar, Australian dollar, Hong Kong dollar, British pound, RMB, Swiss franc;
Accepted payment type: T/T, L/C, D/P D/A, PayPal;
Optional ports: Tianjin, Shanghai, Guangzhou;
Spoken: English, Chinese
6. How can we get your price?
A. We need the following information to quote for you:
1). Product Name
2). standard
3). Material grade (chemical composition)
4). dimension
5). amount
6). Special part drawing