Eigenschaften | Testmethode | Einheit | Typischer Wert | |||||
Dicke | Kincess | μm | 18 | 20 | 25 | 30 | 35 | |
Dickenvariation | Astm-252-78 | % | ± 3 | ± 3 | ± 3 | ± 3 | ± 3 | |
Ertrag | Kincess | m2 /kg | 61,05 | 54,95 | 43,96 | 36,63 | 31,40 | |
AD | ASTM D- 1003 | - | 1,8-2,2 | 1,8-2,2 | 1,8-2,2 | 1,8-2,2 | 1,8-2,2 | |
Zugfestigkeit | MD | ASTM D-882 | Mpa | 130 | 130 | 130 | 130 | 125 |
TD | ASTM D-882 | Mpa | 240 | 240 | 240 | 240 | 240 | |
Dehnung Beim Bruch | MD | ASTM D-882 | % | 200 | 200 | 200 | 200 | 200 |
TD | ASTM D-882 | % | 70 | 70 | 70 | 70 | 70 | |
Reibungskoeffizient O/O | ASTM D-1894 | - | 0,50 | 0,50 | 0,50 | 0,50 | 0,50 | |
Wärmeschrumpfung | MD | ASTM D-1204 | % | 4,0 | 4,0 | 4,0 | 4,0 | 4,0 |
TD | ASTM D-1204 | % | 2,0 | 2,0 | 2,0 | 2,0 | 2,0 |